Print
TEKSLIDE G412
Non-abrasive PTFE compound for softer mating surfaces, such as stainless steel. High resistance to deformation, extremely low coefficient of friction and good thermal and electrostatic dissipation. Use in water reduces the wear rate. Not suggested for using in ultra-dry, vacuum applications, or where electrical insulation is desired.

PRODUCTS

  • Moulded tubes
  • Moulded rods
  • Moulded sheets
  • Extruded tubes
  • Extruded rods
  • Skived tapes
  • Machined parts
  • Piston rings
  • Bearing tapes
 

APPLICATIONS

  • Compressors
  • Pumps
  • Automotive
  • Lip seals
  • Linear Slides

TECHNICAL DATA
SHEET

PROPERTIES UNIT METHOD MOULDED
PHYSICAL - MECHANICAL      
Density
g/cm3
ASTM D792
2,10 - 2,15
Hardness - Shore D
/
ASTM D2240
≥55
Tensile strength CD
N/mm2
ASTM D4745
≥ 15
Elongation at break CD
%
ASTM D4745
≥170
Compressive strength at 1% deformation
N/mm2
ASTM D695
≥6,5
Deformation under load at room temperature 24hours at 13,7 N/mm2
%
ASTM D621
≤10
Permanent deformaton as above after releasing of 24 hours at room temeperature
%
ASTM D621
≤ 6
Dynamic Coefficient of friction ( PV = 0,7 N/mm2 •m/s)
/
ASTM D3702
0,07 - 0,15
Wear factor ( PV = 0,7 N/mm2 •m/s)
μm/h•N/mm2 •m•min
ASTM D3702
0,015 - 0,025
 
 
THERMAL
Service Temperature (min-max)
°C
/
- 200 / + 260
Thermal expansion coefficient (linear) 25 - 100°C
10-5/°C
ASTM D696
12 - 13
 
| + - | RTL - LTR